2026 · Paper 1 · Q6(c)(ii) · p.8
Outline why weld cracks or incomplete fusion may occur during welding.
Marking scheme
Weld cracks may occur from rapid cooling, high residual stress, or using the wrong filler material. They often start at weak points and can spread through the weld. Incomplete fusion happens when the weld metal does not fully bond with the base metal or previous weld passes. This is usually caused by insufficient heat, poor technique or incorrect welding angles.
2026 · Paper 1 · Q6(c)(i) · p.8
Welding defects include porosity, cracking and incomplete fusion. Explain the meaning of weld porosity and outline two methods used to prevent weld porosity occurring. [Diagram: Cross-section of a weld showing porosity, cracking, and incomplete fusion.]
Marking scheme
Weld porosity refers to small holes or gas pockets that form inside a weld, caused by trapped gases during the welding process. This can weaken the strength and quality of the weld. To prevent porosity: Clean the material thoroughly by removing oil, rust, paint and moisture from the metal surface before welding. Use correct shielding methods such as argon gas to protect the weld area from air contamination.
2022 · Paper 1 · Q6(c)(ii) · p.8
Describe the effects of either cracks or spatter on weld strength and finish.
2022 · Paper 1 · Q6(c)(i) · p.8
Outline how weld cracks and slag inclusions may form on a weld. [Image: three examples of weld defects: cracks, inclusions, and spatter.]