2025 · Paper 1 · Q4(a)(i) · p.6
Outline two reasons for surface hardening the plough point. [Image: an agricultural plough.]
Marking scheme
Surface hardening of the plough points will increase the hardness of the outer surface while the core remains relatively soft. This results in the plough point having an increased resistance to both fatigue failure and abrasive wear. (4+4)
2021 · Paper 1 · Q4(a)(i) · p.6
Identify and describe, with the aid of a diagram, the surface hardening process shown.
Marking scheme
Flame hardening The surface of the steel object is heated to 850°C with an oxy-acetylene flame and quenched quickly. This creates a hard outside layer as the heated austenite structure changes to martensite. The depth of hardening depends on the rate of heating. [Diagram: Flame hardening process showing a flame head and water jets directed at the surface of a component.] OR Induction hardening A coil carries high frequency currents which are induced on the surface of the component causing a rapid rise in temperature. This allows a change to austenite in the surface layers of the component. Water jets then cool the steel, transforming the austenite to martensite. This leaves the outer surface hard while the inner core is tough. The frequency of the current determines the depth of heating and the depth of hardening. [Diagram: Induction hardening process showing induction coils surrounding a component, with water spray cooling the surface.] (8)
2019 · Paper 1 · Q3(c) · p.6
Compare flame hardening and induction hardening with reference to the following: • Equipment • Procedures • Quenching.
Marking scheme
Induction hardening: A coil carries high frequency currents which are induced on the surface of the component causing a rapid rise in temperature. This allows a change to austenite in the surface layers of the component. Water jets then cool the steel transforming the austenite to martensite. This leaves the outer surface hard while the inner core is tough. The frequency of the current determines the depth of heating and the depth of hardening. [Diagram: Induction hardening showing component, induction coils, and water spray.] Flame hardening: The surface of the steel object is heated to 850°C with an oxy-acetylene flame and quenched quickly. This creates a hard outside layer as the heated austenite structure changes to hard martensite. The depth of hardening depends on the rate of heating. [Diagram: Flame hardening showing flames, water jets.] (16 marks)