Study notes
No notes have been generated for this topic yet. Open the topic page online and click Generate notes first.
Past exam questions (5)
2017 · Paper 1 · Q2(b)(iii) · p.5
Find the ultimate tensile strength (UTS) of the material. [Visual aid: Table: Load (kN) vs Extension (mm) data for a tensile test.]
Marking scheme
Ultimate tensile strength = Max load/C.S.A. = 181 kN / 113.1 mm² = 1.6 kN/mm²
2017 · Paper 1 · Q2(b)(ii) · p.5
Indicate the following points on your graph: Elastic limit, Start of necking, Fracture point.
Marking scheme
On graph
2017 · Paper 1 · Q2(b)(i) · p.5
The results shown below were obtained from a tensile test on a carbon steel specimen of 12 mm diameter and 80 mm gauge length. Using the graph paper supplied, plot the load-extension diagram. [Table: Load (kN) vs Extension (mm). Load values: 30, 80, 126, 146, 153, 147, 152, 162, 181, 174. Extension values: 0.2, 0.5, 0.8, 0.9, 1.5, 2.0, 2.5, 3.0, 5.6, 8.0.]
Marking scheme
[Graph: A load-extension graph for a material. The x-axis is labeled 'Extension (mm)' from 0 to 8. The y-axis is labeled 'Load (kN)' from 0 to 220. The graph shows an initial linear elastic region up to approximately (1, 120), labeled 'Elastic Limit'. It then shows a region of yielding and strain hardening up to approximately (5, 180), labeled 'Start of Necking'. Finally, it shows fracture at approximately (8, 160), labeled 'Fracture Point'.]
2017 · Paper 1 · Q2(a)(ii) · p.5
Outline, with sketches, the expected results of impact tests on brittle materials and on tough materials. [Visual aid: Image: a Formula 1 car.]
Marking scheme
Tough material: Expect to be more ductile with more plastic deformation and stretching would be expected at the fracture point. Brittle material: A brittle material would expect to be broken or snapped straight across at the notch point. [Image: Two sets of material samples. The top set is labeled 'Tough material' and shows samples that have bent. The bottom set is labeled 'Brittle material' and shows samples that have broken cleanly.]
2017 · Paper 1 · Q2(a)(i) · p.5
The construction of Formula One cars and the materials used are strictly controlled by regulations to maximise the safety of the cars. Front, side and rear impact tests focus on the car's survival cell (cockpit), which must be designed to withstand high impact. Name and describe, with the aid of a diagram(s), a suitable impact testing procedure to examine the suitability of the material used in the survival cell.
Marking scheme
Izod or Charpy notched bar tests are suitable test for toughness. Descriptions of car impact tests will be accepted. Izod Test • 167 joules striking energy. • Test specimen is vertical. • Test piece is clamped at one end. • Test piece notch is facing the pendulum. • The distance the pendulum travels after breaking the piece will give the toughness value. Charpy Test • 300 joules striking energy. • Test specimen is Horizontal. • Test piece is clamped at both ends. • Test piece notch is facing away from the pendulum. • The distance the pendulum travels after breaking the piece will give the toughness value. [Diagram: A Charpy impact test setup showing a scale, starting position of a pendulum hammer, a specimen held on an anvil, and the end of the swing.]