Study notes
No notes have been generated for this topic yet. Open the topic page online and click Generate notes first.
Past exam questions (9)
2025 · Paper 1 · Q4(b)(i) · p.6
Name the transformation line A and the transformation line B. [Diagram: a simplified portion of the iron-carbon equilibrium diagram.]
Marking scheme
A = Upper Critical Temperature Line (UCT) – ferrite starts to form. B = Lower Critical Temperature Line (LCT) - Austenite and cementite to pearlite and cementite transformation, magnetic transformation temperature. (2+2)
2023 · Paper 1 · Q4(b)(iii) · p.6
Compare austenite and pearlite with reference to carbon content, temperature and structure. [Visual aid: Graph: Simplified portion of the iron-carbon equilibrium diagram.]
Marking scheme
Austenite is a high-temperature phase with an FCC crystal structure, forming above the critical temperature and dissolving higher carbon contents (in excess of 0.76% carbon). Pearlite is a BCC microstructure that forms during the eutectoid transformation of austenite and consists of alternating layers of ferrite and cementite. It forms at temperatures below the eutectoid temperature of 723 °C with a carbon content around the eutectoid composition. 6
2023 · Paper 1 · Q4(b)(ii) · p.6
Explain the significance of point D and point E. [Visual aid: Graph: Simplified portion of the iron-carbon equilibrium diagram.]
Marking scheme
D = At the eutectoid point, during the cooling process, the single-phase austenite (γ) transforms into a mixture of two distinct phases: ferrite (a) and cementite (Fe3C). This transformation is known as the eutectoid transformation. It is a crucial process that affects the microstructure and properties of the steel. E = This is a single-phase liquid of 4.3% carbon at the eutectic temperature 1147 °C which converts into solid austenite and cementite. 3+3
2023 · Paper 1 · Q4(b)(i) · p.6
Name the transformation boundary lines A, B and C shown. [Visual aid: Graph: Simplified portion of the iron-carbon equilibrium diagram.]
Marking scheme
A = Liquidus line B = Solidus line C = Eutectoid line / Lower Critical Temperature (LCT) line 2+2+2
2021 · Paper 1 · Q4(b) · p.6
A simplified portion of the iron-carbon equilibrium diagram is shown. [Diagram: A phase diagram showing Temperature (°C) on the y-axis and % Carbon on the x-axis. Regions labelled A, B, C, D. Point X marked at approximately 4.3% Carbon and 1150°C. A horizontal line at 723°C. A region labelled 0.83% carbon steel.]
2015 · Paper 1 · Q3(b)(ii) · p.6
Describe in detail point X and point Y, with reference to each of the following: • Phase change • Composition • Temperature. [Visual aid: Graph: A simplified iron-carbon equilibrium diagram showing regions A, B, C, D and points X, Y. Temperature axis from 200 to 1400 °C, % Carbon axis from 0 to 6%.]
2015 · Paper 1 · Q3(b)(i) · p.6
Name the regions A, B, C and D shown. [Visual aid: Graph: A simplified iron-carbon equilibrium diagram showing regions A, B, C, D and points X, Y. Temperature axis from 200 to 1400 °C, % Carbon axis from 0 to 6%.]
2015 · Paper 1 · Q3(b) · p.6
A simplified portion of the iron-carbon equilibrium diagram is shown. [Graph: A simplified iron-carbon equilibrium diagram showing regions A, B, C, D and points X, Y. Temperature axis from 200 to 1400 °C, % Carbon axis from 0 to 6%.]
2014 · Paper 1 · Q3(b)(i) · p.6
A simplified portion of the iron-carbon equilibrium diagram is shown. Identify the regions A and B. [Diagram: A simplified portion of the iron-carbon equilibrium diagram showing Temperature (°C) on the y-axis and % Carbon on the x-axis. Region A is above the eutectoid line, and Region B is below it, to the right of the eutectoid point.]