2021 · Paper 1 · Q4(c)(iii) · p.6
Upper critical temperature (UCT) and lower critical temperature (LCT).
Marking scheme
The upper critical temperature (UCT) in the iron carbon phase diagram is the “V” shaped line boundary above which solid solution austenite exists. Its “V” point is at 0.83% carbon content called the eutectoid point. The lower critical temperature (LCT) is the horizontal line at 723°C. The LCT is the temperature of the austenite-to-pearlite eutectoid transformation. Below this temperature austenite does not exist and the steel has a layered microstructure.